Method for precompressing flat glass
Abstract
A simple and economical method is described for compacting or shrinking flat glass panes. The method ensures high temperature homogeneity in the glass. First, the glass panes are cleaned and then a stack of glass panes to be treated is assembled without applying a release agent to any of the glass panes. Then the stack of glass panes is placed between ceramic panels made of silicon-infiltrated silicon carbide and this stack together with the ceramic panels is subjected to a heat treatment in a radiation furnace at temperatures ranging from 300° C. to 900° C. The ceramic panels have a thermal conductivity, which, in the region of the heat treatment temperature, is at least 5 times as large as that of the glass panes. The ratio of the total thickness of the ceramic panels to the height of the glass stack should be at least 1/lambd/40W/(mK), wherein lambd is the thermal conductivity of the ceramic panel at the temperatures of the heat treatment.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.