Improvements relating to the recovery of nickel from sulphide ores
Abstract
In a process for extracting nickel and iron, and cobalt if present, as carbonyls from a sulphidic nickel-bearing ore, the preparation of the feed to the volatilizer in which the carbonyls are formed includes concentration of the ore, with, or without, subsequent smelting, to produce a concentrate or matte in which the weight ratio Fe:Ni is less than 10:1, roasting to reduce the S content to 2% or less, and reducing the roasted material with reducing gas to produce a metal-containing product which on treatment with CO yields a mixture of volatilized nickel and iron carbonyls in which the ratio of Fe:Ni is 2:1 to 1:7 and the treatment in the volatilizer is effected under pressure in the presence of active sulphur. The ore is subjected to beneficiation, by froth flotation and magnetic separation, to form a concentrate in which the ratio Cu:Ni is not more than 1:10. The concentrate may be smelted to a matte containing say 10% or more Fe and dead-roasted. The roasted product is reduced at 1300-1600 DEG C. in a controlled atmosphere to convert a maximum proportion of Ni and Co and a controlled proportion of Fe to metal. The controlled atmosphere may be obtained by partial combustion of f
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 9.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.