Case hardening steel e.g. for transmission components of helicopters, competition vehicles and heat engines
Abstract
A case hardening steel, with specified contents of nickel, manganese, copper, cobalt, chromium, molybdenum and vanadium, is new. A novel case hardening steel has the composition (by wt.) 0.06-0.18% C, 0.5-1.5% Si, 0.2-1.5% Cr, 1-3.5% Ni, 1.1-3.5% Mo, \} 1.6% Mn, \} 0.4% V, \} 2% Cu, \} 4% Co, balance Fe and impurities, with the proviso that Ni + Mn + 1.5 Cu + 0.5 Co = 2.5 to 5 wt. % and Cr + Mo + V = 2.4 to 3.7 wt. %. Independent claims are also included for the following: (i) production of case hardened parts by producing the above steel in an arc furnace, subjecting cast ingots to reheating and hot working, carrying out a homogenization and grain refining heat treatment, case hardening and heat treating according to use; (ii) a steel part having the above composition; and (iii) a steel part made by the above process. Preferred Features: The steel has the composition 0.09-0.16 % C, 0.7-1.3 % Si, 0.5-1.2% Cr, 2-3 % Ni, 1.5-2.5% Mo, 0.2-0.7 % Mn, 0.15-0.35 % V, 0.3-1.1 % Cu, \} 1.5 % Co, \} 0.020 % P, \}0.010 % S, \}0.1 % each of Al, Ce, Ti, Zr, Ca and Nb, balance Fe and impurities. Arc furnace melting may be carried out by vacuum induction melting and may be followed by consumable
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 6.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗