Fired porous clay building elements
Abstract
A mould of the desired shape is filled with dried particles of a clay material which foams when fired, and rapidly heated for up to 4 hrs. to 1050-1150 degrees C. The temperature is held for 10-60 mins. so that the particles melt and swell and form a homogenous porous mass which fills the mould. The material is then cooled and the uneven surface sawed, filed or milled to the desired shape and measurement. Pref. the material is used for building stones, blocks, boards, plates and wall elements.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.