Organophilic smectite functionalized with choline for the adsorption of mycotoxins
Abstract
The invention relates to a process for the preparation of a new organophilic smectite comprising the following steps: a) supplying a sodium smectite of sedimentary geological origin; b) treating said smectite with H 2 SO 4 in an amount in the range from 10% to 30% by weight with respect to the smectite dry weight, at a temperature in the range from 20°C to 50°C, to obtain an activated smectite; c) treating said activated smectite with at least one modifying agent consisting of a quaternary ammonium salt of formula [(CH 3 ) 3 N + (CH 2 ) 2 OH] X - , where X - is a monovalent anion, where said modifying agent is at a concentration in the range from 30 to 130 meq/100g to obtain a functionalized smectite; and d) extruding the functionalized smectite to reach an extrudate temperature equal to or higher than 45°C, and drying it at a temperature in the range from 30°C to 80°C. The smectite of the invention acts as an additive and/or supplement capable of sequestering, in vitro, a broad spectrum of mycotoxins and reducing, in vivo, their gastro-intestinal absorption and toxicity (mycotoxicosis).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (2)
Non-Patent Literature (1)
- WILLIAM F. JAYNESRICHARD E. ZARTMAN TOXINS (BASEL, AFLATOXIN TOXICITY REDUCTION IN FEED BY ENHANCED BINDING TO SURFACE-MODIFIED CLAY ADDITIVES, vol. 3, no. 6, June 2011 (2011-06-01), pages 551 - 565