Recycling and reworking method of lithium iron phosphate cathode material
Abstract
A recycling and reworking method of a lithium iron phosphate cathode material is disclosed and includes steps of (a) providing a lithium iron phosphate recycled material; (b) oxidizing the lithium iron phosphate recycled material in an atmosphere at an oxidation temperature ranged from 300°C to 400°C for 1 hour to 5 hours to form a raw material powder composed of LiFePO<sub>4</sub>, Fe<sub>7</sub>(PO<sub>4</sub>)<sub>6</sub>, Fe<sub>2</sub>O<sub>3</sub> and a residual carbon ranged from 0.07 wt.% to 0.6 wt.%; (c) grinding the raw material powder; (d) adjusting the composition of the raw material powder to form a precursor, which has the molar ratio of Li:P = 0.99∼1.05:1, and the molar ratio of Fe:P= 0.98∼1.02:1, wherein a carbon source is added; and (e) heat-treating the precursor in an inert gas at a sintering temperature ranged from 500° C to 800° C for 8 hours to 12 hours to form a lithium iron phosphate regenerated material.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|