Process for preparing a powder of material of natural origin
Abstract
The invention concerns a process for preparing a powder of a material of natural origin, which comprises a step of treating a substance containing at least 70 % by weight of one or more leather wastes in particle form in a twin-screw extruder, wherein a temperature profile is applied that increases from an initial temperature of between 10 and 40°C up to a maximum temperature of between 60 and 120°C, in the presence of water in an amount such that the weight ratio of water to said substance is between 0.20 and 6.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.