Recovering a caustic solution via calcium carbonate crystal aggregates
Abstract
Techniques for converting a portion of a carbonate to hydroxide include receiving an alkaline carbonate solution that includes between 0.1M (moles per liter of solution) to 4.0M hydroxide and between 0.1M to 4.1M carbonate; reacting, in a slaking process, quicklime (CaO) and a low carbonate content fluid to yield a slurry of primarily slaked lime (Ca(OH)2); and reacting the Ca(OH)2 slurry and the alkaline carbonate solution to grow calcium carbonate (CaCO3) crystal aggregates of 0.0005 mm3 to 5 mm3 in volume in a fluidized-bed reactive crystallizer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 1.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.
Non-Patent Literature (1)
- See references of WO 2014164738A2