Ultrahigh-strength multiphase steel having improved properties during production and processing
Abstract
The invention relates to an ultrahigh-strength multiphase steel having a particular composition and also a process for producing a cold- or hot-rolled steel strip of this steel, in which the required multiphase microstructure is generated during continuous heat treatment. According to the invention, the cold- or hot-rolled steel strip is heated in the continuous heat treatment furnace to a temperature in the range from 700 to 950°C and the heat-treated steel strip is subsequently cooled from the heat treatment temperature at a cooling rate of from 15 to 100°C/s to a first intermediate temperature of from 300 to 500°C followed by cooling at a cooling rate of from 15 to 100°C/s to a second intermediate temperature of from 200 to 250°C; the steel strip is subsequently cooled at a cooling rate of from 2 to 30°C/s in air to room temperature or the cooling at a cooling rate of from 15 to 100°C/s is maintained from the first intermediate temperature to room temperature.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 1.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| WO 2021/185514 A1 | Method for producing a rolled multiphase steel strip with special properties | — | 0 |
References Cited — Backward Prior Art (0)
No backward patent references recorded.
Non-Patent Literature (1)
- See references of WO 2013113304A2