Negative electrode for an asymmetric supercapacitor with nickel hydroxide positive electrode and alkali electrolyte and method for manufacturing same
Abstract
The electrode has a continuous current collector whose 50 percent or more than 50 percent of surface exhibits a primary roughness (Ra1) ranging between 0.8 and 15 micrometers measured for a base length ranging between 2 and 200 micrometers. The collector is coated with a mixture of active carbon and a binder. The active carbon has a specific surface area greater than or equal to 500 square meters per gram, and the binder has a mixture of cellulosic compound and a styrenic copolymer. Independent claims are also included for the following: (1) an asymmetric supercapacitor (2) a method for manufacturing an electrode.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 3.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (8)
Non-Patent Literature (2)
- P. P. BHATTACHARJEE ET AL., SCRIPTA MATERIALIA, vol. 56, 2007, pages 13 - 16
- TOMOVICH; PENG; YUAN; YAN: "Laser Scanning, Theory and Applications", article "Quantitative Surface Characterisation Using Laser Scanning Confocal Microscopy"