Sos substrate having low surface defect density
Abstract
The problem of a defect density increase due to lattice constant mismatch between silicon and sapphire is solved, and an SOS substrate having a low defect density is provided. The bonded SOS substrate (8) has a semiconductor thin film (4) provided on the surface of a sapphire substrate (3). The bonded SOS substrate is obtained by means of: a step wherein the sapphire substrate (3) and a semiconductor substrate (1) are provided; a step wherein an ion implanted layer (2) is formed by implanting ions from the surface of the semiconductor substrate (1); a step wherein surface activation treatment is performed to said surface of the sapphire substrate (3) and/or the semiconductor substrate (1) surface having the ions implanted therein; a step wherein the semiconductor substrate (1) surface and the sapphire substrate (3) surface are bonded at 50-350°C; and a step wherein a bonded body (6) is obtained by performing heat treatment at a highest temperature of 200-350°C to the bonded substrate; and a step wherein the bonded body (6) is disposed at a temperature higher than the bonding temperature, visible light is applied toward the ion implanted layer (2) of the semiconductor substrate (1)
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (4)
Non-Patent Literature (1)
- See also references of WO 2010137587A1