Erosion barrier for thermal barrier coatings
Abstract
A workpiece, such as a turbine engine component, comprises a substrate (50), a thermal barrier coating (52) on the substrate (50), and a hard erosion barrier (54) deposited over the thermal barrier coating (52). The erosion barrier (54) preferably has a Vickers hardness in the range of from 1300 to 2750 kgf/mm 2 (12.8 to 27.0 GPa). The erosion barrier (54) may be formed from aluminum oxide, silicon carbide, silicon nitride, or molybdenum disilicide. The erosion barrier (54) may be formed using either an electrophoretic deposition process or a slurry process.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 13.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗