Abstract
Solder is applied to the location to be repaired. Heating melts the solder, following which, it is allowed to set. The solder used, includes the same alloying components as the component being repaired. The proportion of one or more components in the solder, is intentionally varied relative to the corresponding proportion in the component under repair. This variation reduces the melting point of the solder relative to that of the component. The super alloy is nickel- or cobalt-based and contains at least one of Al, Ti, Ta, Cr, Co, Mo, W or Nb, as the main alloying element. The proportion of at least one of Al, Ti, Ta, Nb is raised in the soldering material alloy, relative to that in the superalloy; and/or the proportion of the element W in the soldering alloy is reduced relative to that in the superalloy. Composition ranges are provided for the superalloy, the following composition being a specific implementation expressed in wt% : Cr 12.2, Co 9, Mo 1.9, W 3.8, Ti 4.1, Ta 5, C 0.07, the remainder being Ni. In the corresponding solder, the proportions of Ta and/or Ti are raised by comparison. Setting is allowed to take place at constant temperature, or alternatively, under a tempera
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 4.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (20)
Non-Patent Literature (1)
- S. K. TUNG: "Evolution of nickel borides in Ni-Si-B brazed joints of nickel during post-braze heat treatment", MATERIALS SCI- ENCE AND TECHNOLOGY, vol. 13, December 1997 (1997-12-01), pages 1051 - 1056