Dielectric ceramic composition, dielectric ceramic and laminated ceramic part including the same
Abstract
A dielectric ceramic composition which can be sintered at such a temperature of about 800 to 1000 DEG C as to permit incorporation of and multilayer formation with a low resistant conductor such as Ag or Cu by the simultaneous sintering with the low resistant conductor, which is sintered to form dielectric ceramics having a dielectric constant epsilon r of not more than 10, and a resonator having a large Q x f0 value and an absolute value in temperature coefficient tau f of resonance frequency f0 of not more than 20 ppm/ DEG C, the value being easy to be controlled. The dielectric ceramic composition contains a glass component in an amount of 5 to 150 parts by weight based on 100 parts by weight of a main component represented by general formula: aZnAl2O4-bZn2SiO4-cTiO2-dZn2TiO4, in which the molar fractions of respective components a, b, c, and d satisfy 5.0 </= a </= 80.0 mol%, 5.0 </= b </= 70.0 mol%, 5.0 </= c </= 27.5 mol%, 0 </= d </= 30.0 mol% (a + b + c + d = 100 mol%). <IMAGE>
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 1.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| EP 2,177,490 A4 | Ceramic substrate, process for producing the same, and dielectric-porcelain composition | — | 0 |
References Cited — Backward Prior Art (0)
No backward patent references recorded.
Non-Patent Literature (2)
- No further relevant documents disclosed
- See also references of WO 2004065325A1