Abstract
In accordance with the present invention, there are provided methods for the manufacture of aluminum alloy plates having reduced levels of residual stress, comprising: providing a solution heat-treated and quenched aluminum alloy plate with a thickness of at least 5 inches, and stress relieving the plate by performing at least one compressing step at a total rate of 0.5 to 5 % permanent set along the longest or second longest edge of the plate. In the method, the dimension of the plate where the compression step is performed is along the longest or second longest edge of the plate, which is preferably no less than twice and no more than eight times the thickness of the plate. In further accordance with the present invention, there are provided stress-relieved alloys and plates that are provided with superior Wtot properties as well as reduced residual stress and heterogeneity values.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 2.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.
Non-Patent Literature (1)
- See references of WO 2004053180A3