Method for making an abrasion resistant steel plate and plate obtained
Abstract
The invention concerns a method for making an abrasion resistant steel plate having a chemical composition comprising, by weight: 0.24 % ≤ C ≤ 0.35 %; 0 % ≤ Si ≤ 2 %; 0 % ≤ AI ≤ 2 %; 0.5 % ≤ Si + AI ≤ 2 %; 0 % ≤ Mn ≤ 2.5 %; 0 % ≤ Ni ≤ 5 %; 0 % ≤ Cr ≤< 5 %; 0 % ≤ Mo ≤ 1 %; 0 % ≤W ≤ 2 %; 0.1 % ≤ Mo +W/2 ≤ 1 %; 0 % ≤ B ≤ 0.02 %; 0 % ≤ Ti ≤ 1.1 %; 0 % ≤ Zr ≤ 2.2 %; 0.35 % ≤ Ti + Zr/2 ≤ 1.1 %; 0 % ≤ S < 0,15 %; N <0,03 %, optionally 0 % to 1,5 % of copper; optionally at least one element selected among Nb, Ta and V in contents such that Nb/2 + Ta/4 + V ≤ 0.5 %; optionally at least one element selected among Te, Ca, Bi, Pb in contents not more than 0.1 %; the rest being iron and impurities resulting from the preparation, moreover the chemical composition satisfying the following relationships: 0.095 % ≤ C* = C - Ti/4 - Zr/8 + 7xN/8 and 1.05xMn + 0,54xNi +0.50xCr + 0.3x(Mo + W/2)112 + K > 1.8, with K = 0.5 if B ≤ 0.0005 % and K = 0 if B < 0.0005 %. The method consists in subjecting the plate to a hardening, in rolling heat or after austenitization in a furnace; cooling the plate at a cooling speed higher than 0.5 °C/s between a temperature higher than AC3 and a temperature
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 4.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.
Non-Patent Literature (1)
- See references of WO 2004048619A1