Steel product for high heat input welding and method for production thereof
Abstract
A steel enables to secure a high toughness in a weld heat affected zone in welding performed with a high heat input exceeding 400 kJ/cm, and a manufacturing method enables the steel to be manufactured. The steel has a composition including C: 0.03 to 0.15 mass%; Si: 0.05 to 0.25 mass%; Mn: 0.5 to 2.0 mass%; P: 0.03 mass% maximum; S: 0.0005 to 0.0030 mass%; Al: 0.005 to 0.1 mass%; Ti: 0.004 to 0.03 mass%; N: 0.0020 to 0.0070 mass%; and Ca: 0.0005 to 0.0030 mass%. Individual contents of Ca, O (oxygen), and S satisfy the following expression (1), and the balance of the composition comprises Fe (iron) and unavoidable impurities. 0.3 ≤ ACR ≤ 0.8 where ACR = (Ca - (0.18 + 130 × Ca) × O)/1.25/S, where Ca, O, and S each represent the content (mass%) thereof.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 9.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.