A composite material and method of manufacture involve a mixture of an epoxy resin and a hardener being essentially free of methylenedianiline and vinylcyclohexene dioxide. A fiber reinforcement is located within the matrix. Advantageously, the matrix has a glass transition temperature of at least 250°F (121°C) dry, the resin has a pre-hardening mixed viscosity of 500-1500 cP at 75°F (24°C), and the composite material has, upon hardening, an interlaminar shear strength of at least 6.5 ksi (44.8 N/mm 2 ) dry at 75°F(24°C) and at least 3.5 ksi (24.1 N/mm 2 ) dry at 250°F (121°C).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 6.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • DATABASE WPI Section Ch Week 198833, Derwent World Patents Index; Class A21, AN 1988-230517, XP002316179
  • DATABASE WPI Section Ch Week 199932, Derwent World Patents Index; Class A95, AN 1999-379937, XP002316180