Oxide coated cutting tool
Abstract
SUMMARY The present invention relates to a method of depositing a crystalline α-Al 2 O 3 -layer onto a cutting tool insert by Chemical Vapour Deposition at a temperature of 625-800 °C. The method comprises the following steps depositing a 0.1-1.5 µm layer of TiC x N y O z where x+y+z>=1 and z>0, preferably z>0.2 treating said layer at 625-1000 °C in a gas mixture containing 0.5-3 vol-% O 2 , preferably as CO 2 + H 2 or O 2 + H 2 , for a short period of time about 0.5-4 min, optionally in the presence of 0.5-6 vol-% HCl and depositing said Al 2 O 3 -layer by bringing said treated layer into contact with a gas mixture containing 2-10 vol-% of AlCl 3 , 16-40 vol-% of CO 2 , in H 2 and 0.8-2 vol-% of a sulphur-containing agent, preferably H 2 S, at a process pressure of 40-300 mbar. The invention also includes a cutting tool insert with a coating including at least one α-Al 2 O 3 -layer according to the invention.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 17.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 17 total)
References Cited — Backward Prior Art (0)