A liquid low-sodium silicate forming-solution used for a storage battery, and a container formation method
Abstract
The invention relates to a liquid low-sodium silicate forming-solution used for a storage battery and a container formation method. The forming solution is prepared by mixing 5-15 parts by weight of silica sol containing 40-60wt% SiO2 with 15-25 parts by weight of water, then adding an inorganic acid into the mixture until the PH being 1-4, and magnetizing the mixture in a magnetic field having 1000-6000 gauss for 5-10 minutes to obtain a liquid low-sodium silicate forming-solution with its viscosity being less than 0.02mPas. The liquid low-sodium silicate forming-solution is poured into a battery container. Sequentially, the battery is formed by applying power to the battery at the room temperature for 30∼50 hours. By using the liquid low-sodium silicate forming-solution, a great amount of acid mist is thoroughly keeped from escaping in the period of formation during manufacturing the battery, thus to prevent environment from being polluted and an operator from being harmed. The battery won't generate heat at the time that it is formed, and the battery is sufficiently formed in the shortest time, because the forming solution is a fluid state with good fluidity. The storage bat
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (5)
Non-Patent Literature (1)
- See also references of WO 02101867A1