Pre-expanded polypropylene resin beads and process for producing molded object therefrom by in-mold foaming
Abstract
Pre-expanded polypropylene resin beads which have an expansibility as represented by the following equation of 1.0 to 1.8: Expansibility = [expansion ratio of the beads after steam heating]/[expansion ratio of the beads before steam heating] (wherein the 'expansion ratio of the beads after steam heating' is the value of expansion ratio obtained through heating with steam at the melting peak temperature of the base resin determined by examining the beads with a differential scanning calorimeter). The beads can be molded by various in-mold foaming techniques in a reduced cooling time. Thus, a molded object can be stably obtained from the pre-expanded beads which is satisfactory in fusion bonding between the beads and in surface appearance and has no difference in density between the surface and inner parts thereof.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (4)
Non-Patent Literature (2)
- PATENT ABSTRACTS OF JAPAN vol. 0111, no. 93 (C - 430) 20 June 1987 (1987-06-20)
- See also references of WO 0006636A1