Manufacturing method for hollow stabilizer
Abstract
A manufacturing method for a hollow stabilizer comprises a primary pipe manufacturing process (S1) for subjecting a seam-welded pipe to continuous hot reduction working, thereby obtaining a primary pipe (20a), and winding the primary pipe (20a) in a coil, a cold drawing process (S2) for subjecting the primary pipe (20a) to cold drawing so that the rate of reduction in area is not lower than 30%, thereby obtaining a thick-walled pipe (20b) having a wall thickness ratio of 0.20 to 0.27 higher than that of the seam-welded pipe and tensile strength of 800 N/mm 2 to 1,000 N/mm 2 is obtained, an internal shot peening process (S3) to be carried out as required, a bending process (S4) for bending the thick-walled pipe (20b) into a desired stabilizer shape in a cold state, an annealing process (S5) for subjecting the pipe (20b) to stress relieving annealing at a temperature of 300°C to 450°C, after the bending process (S4), and a shot peening process (S6) for shot-peening the annealed pipe (20b).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 19.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 19 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.
Non-Patent Literature (1)
- None