Production of porous mullite bodies
Abstract
Porous sintered ceramic materials having mullite as its primary phase and a method for producing them are disclosed. The method comprises preparing a plasticizable raw material mixture comprised, by weight, of 75 to 99% pre-reacted mullite powder, and 1.0 to 25% of a water-swelling clay, adding an organic binder system to the mixture and mixing the mixture to form an extrudable mixture, and extruding the mixture to form a substrate of the desired configuration. The green body is dried and fired for a time and at temperature sufficient to form a sintered mullite structure having a narrow through-pore size distribution comprised of pores exhibiting an average intrusion-pore size of between about 2-15 µm, and a total intrusion porosity, as measured by Hg intrusion method, of at least 30%. Inclusion of an amount of alumina or an alumina-yielding precursor in the method results in the formation of a sintered mullite structure exhibiting an acid/base exposure strength loss of less than about 20%.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.