Abstract
A method for improving the SAC process flow includes the deposition of an isolating spacer over the gate stacks after CB liner etch and the removal of previously performed nitride spacer deposition and etching. The isolating spacer is subsequently etched between the stacks to provide sufficient isolation of the bitline contacts from the inserted poly (contact). By depositing an isolating spacer after the typical CB nitride liner etch, additional integrity in the fabricated structures can be achieved.