Polyamide film and polyamide laminate film
Abstract
A polyamide film satisfying (a) a haze value of not more than 5.0%, (b) a coefficient of kinetic friction (A) of not more than 1.0 under 50% humidity, the coefficient (A) being measured with regard to friction between the same two polyamide films, and (c) a ratio of coefficients of kinetic friction (B)/(A) of not more than 1.5, the (B) being a coefficient of kinetic fiction at 65% humidity; a biaxially oriented polyamide film showing an average dimensional change of not more than 3.0% and a difference between the smallest dimensional change and the largest dimensional change of not more than 2.0%, between before immersion in hot water at 95°C and during the immersion, and an average dimensional change of not more than 4.0% and a difference between the smallest dimensional change and the largest dimensional change of not more than 2.0%, between the film without treatment and the film after withdrawal from said hot water; and a polyamide laminate film containing the film as a substrate layer. The films afforded by the present invention have superior properties and are industrially advantageous in abroad range of applications.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 8.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.