Low-k fluorinated amorphous carbon dielectric and method of making the same

0Forward Citations (#75464629 Global)
0.0/yrCitation Velocity (#75464629 Global)
0.56Citation PageRank (#75464629 Global)
3Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

The invention provides a process for depositing fluorinated amorphous carbon (a-F:C) films on IC wafers to provide a low-k interconnect dielectric material. The process, carried out in a PECVD chamber, introduces silane gas (SiH 4 ) into the mixture of C 4 F 8 and CH 4 gases used to deposit a-F:C films. The silane helps to decrease the fluorine etchants in the deposited film, helping to improve the crosslinks in the deposited product. Film produced in accordance with the present invention has both low-k, generally below 2.4, and high thermal stability, generally above 440°C, allowing for higher thermal anneal temperatures.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 0.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (1)

  • YANG H ET AL: "DEPOSITION OF HIGHLY CROSSLINKED FLUORINATED AMORPHOUS CARBON FILM AND STRUCTURAL EVOLUTION DURING THERMAL ANNEALING", APPLIED PHYSICS LETTERS,AMERICAN INSTITUTE OF PHYSICS. NEW YORK,US, vol. 73, no. 11, 14 September 1998 (1998-09-14), pages 1514 - 1516, XP000784064, ISSN: 0003-6951