Heat treatment method for monocrystalline silicon wafers
Abstract
There is disclosed a heat treatment method for a silicon monocrystal wafer comprising the steps of heat-treating in a reducing atmosphere a silicon monocrystal wafer manufactured by growing a silicon monocrystal ingot by Czochralski method characterized in that a wafer obtained from a silicon monocrystal ingot having oxygen concentration of 16 ppma or less which is manufactured by pulling at a growth rate of 0.6 mm/min or more, and in which COPs exist in high density is subjected to anneal heat treatment at 1200 °C or above for one second or more through use of a rapid heating/rapid cooling apparatus, or at 1200 °C or above for 30 minutes or more through use of a batchwise heat treatment furnace, and no defect silicon monocrystal wafer obtained with the method. There can be manufactured a silicon monocrystal wafer in which crystal defects existing on the surface of the wafer or at the surface layer portion thereof are minimized, and there can be provided a silicon monocrystal wafer for a device which is excellent in electric characteristics such as oxide dielectric breakdown voltage and electrical reliability.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 11.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗