Assembling or build-up diffusion brazing method of titanium aluminide workpieces
Abstract
Titanium aluminide parts are diffusion brazed, repaired, surfaced or produced as compact shaped parts using a homogeneous mixture of titanium aluminide powder and titanium or copper based alloy powder having a lower melting temperature and capable of chemically wetting the titanium aluminide powder. A method of joining or repairing titanium aluminide parts by diffusion brazing involves (a) preparing a homogeneous mixture of 40-90 wt.% titanium aluminide powder and 10-60 wt.% titanium or copper based alloy powder having a melting temperature much lower than the incipient fusion temperature of the titanium aluminide powder and capable of chemically wetting the titanium aluminide powder; (b) blending the powder mixture with an organic binder to form a paste; (c) applying the paste to the joint gap or a crack to be repaired; and (d) heating in a vacuum furnace at 1000-1300 degrees C for several minutes to 6 hrs. Independent claims are also included for (i) a method of surfacing a titanium aluminide part by carrying out the above steps (a) and (b), applying the paste to the surface of the part and carrying out the above step (d); (ii) a method of producing a compact shaped element of ti
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 5.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (3)
Non-Patent Literature (1)
- PATENT ABSTRACTS OF JAPAN vol. 18, no. 679 (M - 1728) 21 December 1994 (1994-12-21)