Crystalline polypropylene, process for preparing the same, polypropylene composition, and thermoformed article
Abstract
A crystalline polypropylene which meets the following property requirements (1 to 4), contains a component insoluble in decane at 64 °C, is excellent particularly in hardness and rigidity, and has high melt tension and excellent moldability; a process for preparing the same; and a polypropylene composition and a thermoformed article comprising the above crystalline polypropylene: (1) an intrinsic viscosity [θ] (in decaline at 135 °C) of 0.5 to 10 dl/g; (2) a molecular weight distribution (Mz/Mw) of at least 5 as determined by gel permeation chromatography (GPC; o-chlorobenzene solvent, measurement temp. 140 °C); (3) a pendat isotacticity (mmmm fraction), an index of stereotacticity, of at least 98 % as determined by 13C-NMR spectroscopy; and (4) a D value of at least 4.0 as determined by the equation (I) based on loss tan δ¿0.05? and loss tan δ10 as measured at a temperature of 230 °C under constant strain by means of a melt viscoelasticity measuring instrument at frequencies of 0.05 rad/sec and 10 rad/sec. The number-average molecular weight of the component insoluble in decane at 64 °C is at most 25000.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 2.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (4)
Non-Patent Literature (1)
- See also references of WO 9745463A1