Silicon carbide fabrication
Abstract
An SiC fabrication comprising a CVD-SiC fabrication excellent in strength and thermal characteristics. The SiC fabrication is prepared with a CVD process (i.e. CVD-SiC fabrication) which has a thermal conductivity along the direction of the SiC crystal growth between 100 and 300 W/m·K, and an average grain diameter of the internal structure between 4 to 12 µm. It is preferred that the ratio of the thermal conductivity along the direction of the SiC crystal growth to the thermal conductivity in the perpendicular direction is in a range of 1.10 to 1.40.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (6)
Non-Patent Literature (1)
- DATABASE WPI Section Ch Week 9444, Derwent World Patents Index; Class K05, AN 94-354500, XP002090598