Tempered glass, a quenching method for a glass sheet and a quenching apparatus for a glass sheet
Abstract
In a tempered glass comprising a glass sheet having a thickness of 2.3-3.5 mm in which an average surface compressive stress of 1000-1300 kg/cm 2 is formed, the tempered glass being characterized in that: there are formed a plurality of mutually parallel belt-like regions A having a width of 10-30 mm and a plurality of belt-like regions B each being interposed between adjacent belt-like regions A in the glass sheet; in the belt-like regions A, there are a plurality of reference points a having a principal stress difference of 120 kg/cm 2 or less, which is larger than principal stresses at peripheral areas of the reference points a , wherein directions of principal stresses at the reference points a are mutually in substantially parallel; there exists no point having a larger principal stress difference than principal stress differences between adjacent reference points a ; and the shortest lines connecting adjacent reference points a form the center line, as the reference line, of each of the belt-like regions A; and in the belt-like regions B, there are a plurality of reference points b which have a larger principal stress difference than principal stress differences at any periph
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 6.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.