Sputter deposition and annealing of copper alloy metallization M
Abstract
A copper metallization structure and its method of formation in which a layer (100) of a copper alloy, such as Cu-Mg or Cu-Al is deposited over a silicon oxide based dielectric layer (64) and a substantially pure copper layer (102) is deposited over the copper alloy layer (100). The copper alloy layer (100) serves as a seed or wetting layer for subsequent filling of via holes (66) and trenches with substantially pure copper and also provides barriers at the interfaces with the underlying dielectric and the overlying pure copper. The copper alloy may be deposited cold in a sputter process, but, during the deposition of the pure copper layer (102) or afterwards in a separate annealing step, the temperature is raised sufficiently high to cause the alloying element of the copper alloy to migrate to the dielectric layer (64). Alternatively, the copper alloy may be deposited with the wafer held at an elevated temperature. The alloying element that has migrated to the oxygen-rich surfaces oxidizes to form thin stable layers (70), for example of magnesium or aluminum oxide, that act as barriers there against diffusion of copper into and through the dielectric layer (64). The inner barrier
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 9.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.