Method for surface treatment, an ornament and a device
Abstract
When machine works such as a honing processing, nicking processing or mirror finishing are applied on the surface 10a of the facing member of watches and clocks composed of Ti and Ti alloy, a layer of Ti oxide is formed to cause surface blackening. This oxide layer or other foreign substances are eliminated, for example, by a chemical etching or electropolishing by immersing in a etching solution, followed by forming a transparent protective layer on the surface 10a by coating, for example, with a glass coating solution and drying. The etching solution described above preferably comprises a mixed solution containing HF, HNO 3 and H 2 SO 4 . The arrangement prevents the surface of Ti and Ti alloy from contamination with fingerprints and being scratched, as well as enhancing the degree of whiteness and improving the quality of appearance.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 3.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.