Degradable monofilament and preparation process thereof
Abstract
The invention is a degradable copolymer filament comprising an internal structure separating into, (a) a matrix phase comprised as a primary component of a polymer segment which exhibits a tensile Young's modulus of 2GPa or less and a strength retention of 50% or more after two weeks in water at 37°C, pH 7.3, and (b) a micro-dispersed phase comprised as a primary component of a polymer segment which exhibits a tensile strength of 200MPa or more and a strength reduction greater than the matrix phase in water at 37°C, pH 7.3, a weight ratio of each component in the matrix phase and dispersed phase being 50 : 50 to 95 : 5, respectively, and the dispersed phase having a needle-like structure oriented by stretching to the fiber direction. The invention can provide a degradable monofilament having an excellent mechanical strength and flexibility, moderate hydrolyzability, high ligature stability and being suitable as a material of surgical absorbable suture and a preparation process of the same.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 6.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.