EP 0,807,965 A2#5555508 Most CitedPendingEuropean Patent Office (EPO)Application

Method of manufacturing layered ferroelectric Bi containing film

16Forward Citations (#5555508 Global)
0.6/yrCitation Velocity (#14474494 Global)
5.34Citation PageRank (#2975188 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

A method of forming a Bi-layered ferroelectric thin film on a substrate with good reproducibility, using a mixed composition of a Bi-containing organic compound and a metal polyalkoxide compound by at least one technique selected from the group consisting of molecular deposition such as CVD, and spincoat-sintering. <IMAGE>

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 16.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 16 total)

PatentTitleYearCitations
US 6,495,878 B1Interlayer oxide containing thin films for high dielectric constant application200262
KR 20030042482 AChemical solution of bismuth lanthanum titanate for ferroelectric thin film—2
US 5,972,096 ACoating solutions for use in forming bismuth-based ferroelectric thin films19999
US 6,867,452 B2Interlayer oxide containing thin films for high dielectric constant application of the formula AB2O6 or AB2O720057
WO 0,034,549 A3Cvd process using bi alcoxides—0
US 6,303,231 B1Coating solutions for use in forming bismuth-based ferroelectric thin films, and ferroelectric memories formed with said coating solutions, as well as processes for production thereof200165
GB 2,358,396 APrecursors for growth of heterometal-oxide films by MOCVD—0
WO 0,077,832 A3Metal oxide thin films for high dielectric constant applications—2
WO 0,000,497 A1Precursors for growth of heterometal-oxide films by mocvd—1
US 6,120,912 ACoating solutions for use in forming bismuth-based ferroelectric thin films, and ferroelectric thin films, ferroelectric capacitors and ferroelectric memories formed with said coating solutions, as well as processes for production thereof20009
GB 2,358,396 BPrecursors for growth of heterometal-oxide films by MOCVD20030
EP 0,878,837 A3Ferroelectric thin film comprising a bufferlayer and a Bismuth layered compound—0
US 6,500,489 B1Low temperature CVD processes for preparing ferroelectric films using Bi alcoxides200212
US 6,485,784 B1Precursors for growth of heterometal-oxide films by MOCVD20028
EP 0,854,503 A1Coating solutions for use in forming bismuth-based ferro-electric thin films, and ferro-electric thin films, ferro-electric capacitors and ferro-electric memories formed with said coating solutions, as well as processes for production thereof—5

References Cited — Backward Prior Art (0)

No backward patent references recorded.