Heat resisting steel and steam turbine rotor shaft
Abstract
Disclosed is a heat resisting steel whose metal structure is entirely martensite phase produced by tempering after quenching. The steel comprises, by weight, 0.05 to 0.20% C, not more than 0.15% Si, not more than 1.5% Mn, not more than 1.0% Ni, 8.5 to 13.0% Cr, not more than 3.50% Mo, not more than 3.5% W, 0.05 to 0.30% V, 0.01 to 0.20% Nb, not more than 5.0% Co, 0.001 to 0.020% boron, 0.005 to 0.040% nitrogen, 0.0005 to 0.0050% oxygen and 0.00001 to 0.0002% hydrogen. The steel has preferably not more than 10 of the Cr equivalent. The steel has 10 kgf/mm 2 or more of 100000 hours creep rupture strength at 650°C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 16.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 16 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (1)
- PATENT ABSTRACTS OF JAPAN vol. 009, no. 036 (C - 266) 15 February 1985 (1985-02-15)