Propylene homopolymer
Abstract
A polypropylene homopolymer is characterised by a broadened molecular weight distribution, i.e. M w /M n is 7-50, and by a compression-moulded flexural modulus of at least 285 kpsi (1965 MPa); an injection-moulded flexural modulus of at least 245 kpsi (1482 MPa); a tacticity of at least 96.5%; a melt flow rate of at least 0.1 up to 200 grams per 10 minutes; a melting point in the range of 160°C to 168°C; a heat of fusion of at least 24 calories per gram; and less than 2% by weight of hexane extractables as measured by a 3 hour extraction.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 42.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 42 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.