Ethylene type quaternary copolymer rubber
Abstract
The present invention provides an ethylene type quaternary copolymer rubber which is formed when ethylene, an α-olefin, a non-conjugated diene, and a vinylidene aromatic monomer are polymerized. More specifically, it relates to an ethylene type quaternary copolymer having a low crystallinity which can be easily bonded and blended with a diene type rubber and to which such properties as mechanical strength, abrasion resistance, and resistance to dynamic fatigue can be effectively imparted. The quaternary copolymer rubber in accordance with the present invention has characteristics that (1) the non-conjugated diene has a content of 0.1 to 10 mol%; (2) the vinylidene aromatic monomer has a content of 0.1 to 45 mol%; (3) the limiting viscosity [η] measured at 70°C in xylene is 0.5 to 10 dl/g; (4) the glass transition temperature (Tg) measured by a differential scanning calorimeter (DSC) is a single value and not higher than 0°C; and (5) the portion soluble to methyl ethyl ketone is not greater than 2% by weight.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 12.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (12 of 12 total)
References Cited — Backward Prior Art (2)
Non-Patent Literature (2)
- MCRAE M.A. ET AL.: "Die Makromolekulare Chemie", vol. 177, 1976, pages: 461
- TAKAYAMA AND USAMI: "Characterization of Polyethylene by Infrared Absorption Spectrum"