Process for forming a dielectric film and a capacitive structure in microelectronic devices
Abstract
A semiconductor device and process for making the same are disclosed which incorporate a relatively large percentage of holmium dopant (0.3% to 3%) into a BST dielectric film 24 with small grain size (e.g. 10 nm to 50 nm). Dielectric film 24 is preferably disposed between electrodes 18 and 26 (which preferably have a Pt layer contacting the BST) to form a capacitive structure with a relatively high dielectric constant and relatively low leakage current. Apparently, properties of the thin film deposition and small grain size, including temperatures well below bulk BST sintering temperatures, allow the film to support markedly higher defect concentrations without holmium precipitation than are observed for bulk BST. For holmium doping levels generally between 0.3% and 3% (compensated with titanium and/or manganese), better than 50% improvement in dielectric constant and two to six orders of magnitude reduction in leakage current (compared to undoped BST) have been observed for such films.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 2.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.
Non-Patent Literature (1)
- None