Patents
EP 0,701,002 A1#1726377 Most CitedPendingEuropean Patent Office (EPO)Application

Process for moulding aluminium- or magnesiumalloys in semi-solidified state

35Forward Citations (#1726377 Global)
1.2/yrCitation Velocity (#5248221 Global)
9.86Citation PageRank (#1086805 Global)
5Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

The melt of a magnesium or an aluminum alloy that have a composition within maximum solubility limits is poured into a billet-forming mold at a selected temperature exceeding the liquidus line of the alloy but not higher by more than 30°C and the melt is cooled to solidify at a cooling rate of at least 1.0°C/sec over the solidification zone so as to form a billet and, thereafter, the billet is heated at a rate of at least 0.5°C/min through the range bound by the solubility line and the solidus line of the alloy and further heated to a given temperature above the solidus line of the alloy and held at that temperature for 5 - 60 minutes, thereby spheroidizing the primary crystals and, thereafter, the billet is further heated to a given molding temperature below the liquidus line of the alloy and the semi-solid billet is fed into a shaping mold and shaped under pressure. Alternatively, the melt of a hypo-eutectic aluminum alloy having a composition at or above maximum solubility limits is poured into a billet-forming mold at a selected temperature exceeding the liquidus line of the alloy but not higher by more than 30°C and the melt is cooled to solidify at a cooling rate of at least

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 35.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗