Patents
EP 0,645,181 A2#7526249 Most CitedPendingEuropean Patent Office (EPO)Application

Method of improving the contaminant resistance of a smectite clay

13Forward Citations (#7526249 Global)
0.4/yrCitation Velocity (#19194771 Global)
2.65Citation PageRank (#9242116 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

There is disclosed a method of treating a water-swellable clay after the clay has been mined and dried to improve its properties when in contact with contaminated water. After the common initial drying of the clay to a moisture content of 12% by weight or less, the clay is impregnated with an aqueous solution containing a dissolved, water-soluble polymer, in an amount of at least about 0.5% by weight based on the dry weight of the clay, and the clay is wetted to a moisture content of more than 12% by weight, preferably at least about 15% or more, based on the dry weight of the clay, and then redried to a moisture content of 12% by weight or less, based on the dry weight of the clay. This rewetting step to hydrate and polymer-impregnate the clay, and then redrying the clay, unexpectedly improves the contaminated water absorbency, and viscosity properties when the clay is in contact with contaminated water; unexpectedly increases the rheology properties of the clays for oil well drilling fluids and lost circulation fields when contaminated water is encountered during drilling, enhances the clay properties when used as a suspending agent in the cosmetics and pharmaceutical industries

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 13.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (13 of 13 total)

PatentTitleYearCitations
US 8,846,796 B2Method of producing a modified smectite or smectite-containing substance capable of taking up and releasing water in a reversible manner20140
CN 102,284,274 APreparation method for modified montmorillonite adsorbent and application thereof to removing micro or trace iodine—12
EP 2,668,345 B1Improved bentonite barrier compositions and containment comprising said compositions20152
EP 1,985,586 A1Method of producing a modified smectite or smectite-containing substance capable of taking up and releasing water in a reversible manner—3
EP 2,668,344 B1Geosynthetic clay liners comprising bentonite barrier compositions for use in containment applications20150
US 8,318,616 B2Salt water swellable compositions and articles20121
WO 2008/133497 A3Method of producing a modified smectite or smectite-containing substance capable of taking up and releasing water in a reversible manner—0
EA 026,671 B1Method of producing a modified smectite or smectite-containing substance capable of taking up and releasing water in a reversible manner—0
AU 2010284574 B2Salt water swellable compositions and articles20140
CN 113,877,521 APreparation method and application of clay/tannin/metal ion composite material for efficiently adsorbing antibiotics—13
AU 2008244775 B2Method of producing a modified smectite or smectite-containing substance capable of taking up and releasing water in a reversible manner20130
WO 2011/022134 A1Salt water swellable compositions and articles—5
EP 0,808,568 A1Intercalates and exfoliates formed with organic pesticide compounds and compositions containing the same—4

References Cited — Backward Prior Art (0)

No backward patent references recorded.