Alcaline cyanide baths for electroplating copper-tin alloys coatings
Abstract
To produce bright to glossy, planarised copper-tin alloy coatings, electroplating baths are used which contain from 1 to 60 g/l of copper as copper cyanide, from 1 to 50 g/l of tin as alkali metal stannate, from 0 to 10 g/l of zinc as zinc cyanide, from 1 to 100 g/l of free alkali metal cyanide, from 1 to 50 g/l of free alkali metal hydroxide and, as a complexing agent, from 1 to 200 g/l of oligosaccharides and/or polysaccharides as well as, additionally, from 0.01 to 4 g/l of alkene sulphonate, alkine sulphonate, pyridine compounds or sulphur-containing propane sulphonates as a brightener.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 10.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.