Low temperature chemical vapor deposition and method for depositing a tungsten silicide film with improved uniformity and reduced fluorine concentration
Abstract
A tungsten silicide (WSix) film is formed by chemical vapor deposition using the reduction of tungsten hexafluoride (WF6) with dichlorosilane (SiH2Cl2) referred to as DCS and a reducing agent comprising silane (SiH4), hydrogen, or a mixture thereof. According to the method of the present invention, the WSix film is formed in a CVD reactor operating at a low pressure and at a wafer temperature between about 300 and 550°C. In the preferred embodiment, a thin nucleation layer is deposited before the WSix film. The deposited WSix films exhibit low flourine concentrations with good within-wafer uniformity and process stability. The attached plot illustrates a comparison the growth rates (given as the weight in mg per deposition time in Min) versus the wafer temperature in °C, using DCS (curve 10), DCS + SiH₄ (curve 12) and DCS + H2 (curve 14).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 19.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 19 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.