Blister-resistant steel sheet and method for production thereof
Abstract
Blister-resistant steel sheet consists essentially of 0.0005 to 0.003wt.% C, 0.10 to 2.2wt.% Mn, 0.6wt.% or less Si, 0.07wt.% or less P, 0.025wt.% or less S, 0.02 to 0.06wt.% of sol. Al, 0.0035wt.% or less N, 0.003wt.% or less O, [(48/14)N + (48/32)S + 4 x (48/12)C] wt.% or less Ti and the balance being Fe and inevitable impurities; and smaller one of either Ti (wt.%) or [(48/14)N + (48/32)S] (wt.%) being [0.002 t² + 0.003] or more, where t is a thickness (mm) of the steel sheet. Method for producing blister-resistant steel sheet comprises preparing a cold rolled steel sheet having the composition of described above, and continuously annealing or continuous hot dip galvanizing by heating the steel sheet from room temperature to 650 - 720°C at a rate of 20°C/sec or more and further to the soaking temperature above recrystallization temperature at a rate of 1 - 5°C/sec.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 4.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗