Process for preparing an ingot of high critical temperature superconducting oxide
Abstract
Process for the manufacture by melting-solidification of an ingot made of superconductive oxide with a high critical temperature, belonging especially to the classes YBaCuO, BiSrCaCuO, TlBaCaCuO, characterised in that the starting point is an ingot (1) of oxide which has the appropriate stoichiometry, which is held horizontally by levitation on a gas film inside a furnace (40), that it is melted, that a vertical temperature gradient is established in the said furnace so that a nucleation begins in the lower part of the said ingot, that, while the said temperature gradient is maintained, the overall temperature of the furnace is lowered at a rate lower than or equal to 0.1 DEG C/hour to the temperature corresponding to a complete solidification, and in that finally a conventional oxygenation treatment is applied to the said ingot. <IMAGE>
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 8.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.