Abstract
In a method of coating or sealing electronic components and component groups using single-component reactive resin mixtures which are storage-stable at room temperature for several months, reactive resin mixtures are used which contain the following components: - a cationically curable solvent-free epoxy resin, - a triarylsulphonium salt with hexafluorophosphate, hexafluoroarsenate or hexafluoroantimonate as anion, in a proportion of 0.01 to 5% by weight (based on epoxy resin) and - a benzylthiolanium salt with hexafluorophosphate, hexafluoroarsenate or hexafluoroantimonate as anion, in a proportion of 0.01 to 5% by weight (based on epoxy resin), and - conventional additives if required. These reactive resin mixtures are cured by UV radiation and heat.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.