Process for manufacturing galvanized steel sheet by nickel pre-coating method
Abstract
Process for manufacturing a galvanized steel sheet, comprising steps of coating a steel sheet with nickel in an amount of from 0.2 to 2 g/m², heating the steel sheet thus coated to a temperature within the range of from 420°C to 500°C in a non-oxidative atmosphere, and dipping the nickel coated steel sheet into a molten zinc bath containing aluminum at a content of from 0.1 to 1% without contact with air, wherein the steel sheet is dipped into the molten zinc bath within 15 seconds after the temperature of the steel sheet exceeds 350°C in the heating step, and apparatus for performing the process. The galvanized steel sheet has superior surface appearance and coating adherence.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 8.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.