Process and apparatus for fabrication of silver coated high temperature ceramic superconductor fiber with metal substrate
Abstract
A method and apparatus for manufacturing a superconductor wire has a wire take-up spool (16) and a feed speed control spool (12). A wire substrate (22) is taken from the feed speed control spool (12) and onto the take-up spool (16) as the wire take-up spool (16) is rotated. The wire (22) passes through a container (36) which holds a diffusion barrier material (50), where the diffusion barrier material (50) is electrophoretically deposited onto the wire substrate (22) and subsequently sintered. The wire (22) is also passed through a container (36a) which holds a superconductor material suspended in solution (38a), and a layer of the superconductor material (70) is electrophoretically deposited onto the diffusion barrier (50). The grains of the superconductor layer (70) are then magnetically aligned and sintered. Also, a silver coating (76) is electrophoretically deposited onto the superconductor layer (70) and sintered. A diffusion bonding inhibitor material (78) is then applied to the silver coating (76). Then, the silver-coated superconductor wire is spooled and heated to 400°C for one day to oxidize the superconductor layer (70).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 8.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.