Process for forming refractory metal silicide layers in an integrated circuit
Abstract
A method for forming reactive metal silicide layers at two spaced locations on a silicon substrate, which layers can be of different thicknesses and/or of different reactive metal is provided. A silicon substrate (10) has a silicon dioxide layer (14) formed thereon followed by the formation of a polysilicon layer (16) on the silicon dioxide layer (14), followed by forming layer of refractory metal (18), e.g. titanium on the polysilicon (16). A non-reflecting material (20), e.g. titanium nitride is formed on the refractory metal (18). Conventional photoresist techniques are used to pattern the titanium nitride (20), the titanium (18) and polysilicon (16), and the titanium (18) is reacted with the contacted polysilicon (16) to form a titanium silicide (24). The portion of silicon dioxide (14) overlying the silicon substrate is then removed and the exposed substrate is ion implanted to form source/drain regions (27). A second layer of refractory metal (28), either titanium or some other refractory metal, is deposited over the source/drain region (27), and either over the titanium nitride (20), or over the first formed silicide (24) by first removing the titanium nitride (20). The seco
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 33.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 33 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.