Lithiated nickel dioxide and secondary cells prepared therefrom
Abstract
Lithiated nickel dioxide cathode-active materials for electrochemical cells having the formula Li x Ni 2-x-y M y O₂, with x being between about 0.8 and about 1.0, M being one or more metals selected from cobalt, iron, chromium, titanium, manganese and vanadium, and y being less than about 0.2, with the proviso that y is less than about 0.5 for cobalt, which material is substantially free of lithium hydroxide and lithium carbonate. The materials are prepared by providing a substantially homogeneous dry intermediate mixture of a starting material containing a nickel compound selected from nickel oxide, nickel hydroxide, and mixtures thereof, and optionally including one or more oxides or hydroxides of a transition metal selected from cobalt, iron, chromium, titanium, manganese and vanadium, together with between about a 10 and about a 25% stoichiometric excess of lithium hydroxide. The mixture is heat treated at a temperature above about 600°C in an atmosphere substantially free of carbon dioxide and having a partial pressure ratio of oxygen to water vapor greater than about 15, after which any lithium hydroxide or lithium carbonate present in the mixture is removed. Thermally stable
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 45.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 45 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.